| Uncoated carbon steel | Low in the presence of moisture and oxygen; rusts readily without protection. | Dry indoor locations or settings where a suitable coating and maintenance program can be maintained. | Usually needs paint, a protective coating, or another corrosion-control system for exposed service. Scratches and damaged coatings can expose the steel. | Frames, supports, machinery, and structural components in controlled or protected environments. |
| Hot-dip galvanized steel | Zinc coating provides a barrier and sacrificial protection to exposed steel at small coating defects. | Many outdoor and moderately corrosive environments, depending on coating thickness, exposure, and maintenance. | Coating life varies with atmospheric conditions. Prolonged contact with strongly acidic or alkaline substances can damage zinc; fabrication after galvanizing may require coating repair. | Outdoor platforms, guardrails, support structures, and general-purpose exterior components. |
| Weathering steel | Can develop a relatively protective rust patina when exposed to appropriate wet-dry cycles. | Locations with good drainage and alternating periods of wetting and drying, away from persistent dampness and heavy salt exposure. | Not suitable for every climate. Continuous moisture, trapped water, marine salt, or de-icing salts can prevent a stable protective patina from forming. | Bridges, façades, and outdoor structures designed for suitable exposure conditions. |
| Type 304 stainless steel | Good general atmospheric and indoor corrosion resistance; vulnerable to chloride-induced pitting and crevice corrosion. | Clean indoor environments, food-handling areas, and many non-marine outdoor applications with limited chloride exposure. | Salt deposits and stagnant moisture can increase localized corrosion risk. Welding and surface condition can affect performance. | Indoor equipment, architectural components, tanks, and general-purpose fabricated parts. |
| Type 316 stainless steel | Generally more resistant than Type 304 to chloride-related pitting and crevice corrosion because it contains molybdenum. | Coastal atmospheres and applications with moderate chloride exposure, subject to proper design, cleaning, and exposure assessment. | Not immune to seawater corrosion, especially in crevices or stagnant conditions. Performance depends on chloride concentration, temperature, and surface details. | Marine-adjacent fittings, chemical-processing equipment, and exterior components exposed to salt spray. |
| Duplex stainless steel (e.g., 2205) | High strength and generally strong resistance to pitting and stress-corrosion cracking in chloride-containing environments. | More demanding chloride service than common austenitic stainless grades, when the specific environment and design are properly evaluated. | Requires suitable welding procedures and control of heat input to preserve properties. It is not universally resistant to all acids or seawater conditions. | Process equipment, pressure-containing components, and structural parts in demanding industrial environments. |
| Aluminum alloy 5052 | Good resistance to atmospheric and many marine environments due to its protective oxide film; can be affected by galvanic contact. | Marine and outdoor applications where low weight is valuable and the alloy is compatible with the service conditions. | Electrical contact with dissimilar metals in the presence of an electrolyte can accelerate galvanic corrosion. Strength and weld design must be considered. | Marine panels, enclosures, transport components, and lightweight fabricated structures. |