| 42CrMo4 / AISI 4140 alloy steel | Quenched and tempered; commonly supplied around 28–32 HRC, with tensile strength often approximately 900–1,100 MPa. Actual values depend on section size and tempering condition. | Offers a useful balance of strength, toughness, hardenability, and machinability for loaded components. | Check the material certificate, heat-treatment record, hardness readings, and tensile-test results against the specified condition and standard. | Shafts, gears, connecting components, bolts, and machine parts. |
| 34CrNiMo6 / AISI 4340-type steel | Quenched and tempered; strength and hardness vary substantially with tempering. High-strength conditions may reach roughly 1,000–1,400 MPa tensile strength. | Nickel, chromium, and molybdenum support hardenability and toughness in demanding, heavily loaded parts. | Confirm the specified grade, heat-treatment condition, tensile properties, hardness, and—where required—impact-test results. | Heavy-duty shafts, high-strength fasteners, landing-gear components, and large machinery parts. |
| 20MnCr5 / 16MnCr5 case-hardening steel | After carburizing and hardening, the surface is commonly about 58–62 HRC; the core is intentionally softer and tougher. Case depth is specified for the part and process. | A hard, wear-resistant surface combined with a tougher core helps gears and similar parts resist surface wear and impact. | Measure surface hardness and effective case depth; inspect the core condition and verify the carburizing and quenching records. | Gears, pinions, splined shafts, and other components requiring a hardened wear surface. |
| 100Cr6 / AISI 52100 bearing steel | Hardened bearing components commonly reach approximately 60–66 HRC. Cleanliness, carbide distribution, and heat treatment are critical. | High hardness and suitable microstructure support rolling-contact fatigue resistance and dimensional stability. | Review hardness and metallographic results; for critical bearings, specify cleanliness and inclusion-control requirements. | Rolling-element bearings, races, and precision wear components. |
| Hardness and hardness uniformity | Specified by grade, heat treatment, part geometry, and service conditions; no single hardness value suits every alloy steel part. | Hardness affects wear resistance and strength, while excessive hardness can reduce toughness or increase cracking risk. | Use calibrated Rockwell, Brinell, or Vickers testing as appropriate; take measurements at defined locations and depths. | Alloy steel parts subject to wear, contact stress, or repeated loading. |
| Toughness and impact resistance | Specified using an agreed test method, temperature, and minimum acceptance value; results depend on material condition and orientation. | Helps a part resist fracture under shock, notches, low temperatures, or fluctuating loads. | Request Charpy impact results when relevant and verify that specimen orientation and test temperature match the specification. | Drive components, pressure-loaded parts, heavy equipment, and safety-critical components. |
| Dimensional accuracy and surface finish | Tolerances and roughness should be defined on the engineering drawing; achievable values depend on geometry and manufacturing process. | Correct dimensions and finish support fit, assembly, sealing, and fatigue performance. | Check inspection reports, calibrated gauges or coordinate-measuring results, and surface-roughness measurements against drawing requirements. | Precision shafts, gears, bearing seats, hydraulic parts, and fitted assemblies. |
| Material traceability and process control | Heat or batch identification should link the part to its material certificate and relevant manufacturing and heat-treatment records. | Traceability makes it possible to confirm composition, processing history, and compliance with the purchase specification. | Review material test certificates, batch identification, inspection records, and documented nonconformance controls. | Parts requiring documented quality assurance or controlled production. |
| Data note: The property figures shown are typical indicative ranges, not guaranteed values. Actual results vary with the applicable material standard, product size, heat treatment, sampling location, and test method. Confirm acceptance limits in the part drawing or purchase specification. |